High temperature volatilization of neodymium from thorium carbide particles
High temperature volatilization of neodymium from thorium carbide particles
itial decontamination of Thorium carbide from isotopes of Neodymium ias been obtained by heating under vacuum at temperatures in the range 2000 - 2800 ° C. Sol-gel processes have been adopted to prepare Thorium carbide spherical particles containing 200 or 1000 ppm of Neodymium. Nd$^{147}$ ($\tau$$...
Saved in:
Personal Name(s): | Podo, L. A. |
---|---|
Nickel, Hubertus | |
Contributing Institute: |
Publikationen vor 2000; PRE-2000; Retrocat |
Imprint: |
Jülich
Kernforschungsanlage Jülich GmbH Zentralbibliothek, Verlag
1967
|
Physical Description: |
17 p. |
Document Type: |
Report Book |
Research Program: |
Addenda |
Series Title: |
Berichte der Kernforschungsanlage Jülich
502 |
Link: |
OpenAccess |
Publikationsportal JuSER |
itial decontamination of Thorium carbide from isotopes of Neodymium ias been obtained by heating under vacuum at temperatures in the range 2000 - 2800 ° C. Sol-gel processes have been adopted to prepare Thorium carbide spherical particles containing 200 or 1000 ppm of Neodymium. Nd$^{147}$ ($\tau$$_{1/2}$ = 11 .1 d, $\gamma$ = 0.53 MeV) was used as a tracer for radiometric determinations . |