Thermal Recovery of the Electrochemically Degraded LiCoO 2 /Li 7 La 3 Zr 2 O 12 :Al,Ta Interface in an All-Solid-State Lithium Battery
Thermal Recovery of the Electrochemically Degraded LiCoO 2 /Li 7 La 3 Zr 2 O 12 :Al,Ta Interface in an All-Solid-State Lithium Battery
Saved in:
Personal Name(s): | Ihrig, Martin (Corresponding author) |
---|---|
Kuo, Liang-Yin / Lobe, Sandra / Laptev, Alexander M. / Lin, Che-an / Tu, Chia-hao / Ye, Ruijie / Kaghazchi, Payam / Cressa, Luca / Eswara, Santhana / Lin, Shih-kang / Guillon, Olivier / Fattakhova-Rohlfing, Dina (Corresponding author) / Finsterbusch, Martin (Corresponding author) | |
Contributing Institute: |
Werkstoffsynthese und Herstellungsverfahren; IEK-1 JARA-ENERGY; JARA-ENERGY |
Published in: | ACS applied materials & interfaces, 15 (2023) 3, S. 4101 - 4112 |
Imprint: |
Washington, DC
Soc.
2023
|
DOI: |
10.1021/acsami.2c20004 |
DOI: |
10.34734/FZJ-2024-01927 |
Document Type: |
Journal Article |
Research Program: |
Components and Cells |
Link: |
OpenAccess |
Publikationsportal JuSER |
Please use the identifier: http://dx.doi.org/10.34734/FZJ-2024-01927 in citations.
Description not available. |